Appearance: Black ball φ (2 ~ 6) mm
Description of Deoxidization catalyst 506HL type
1 As soon as it is filled with purify air, it can be put into use.
2 For a period of time after using this catalyst, once the effect of deoxidizing by soaking water drop or failure, and heating to 200 degrees Celsius regeneration.
3 Its use of temperature cannot exceed 45 ° c.
4 The catalyst should avoid contact with chloride and sulfides, in case of failure of poisoning.
Application:It is used for carbon dioxide, argon oxygen as hydrogenation of inert gases.